The Materials Data Facility

Discover Data

Search Results

A ground truth dataset for anomaly detection on load-displacement nanoindentation curves for NiFe electroplated samples

Henriksen, Amelia; Zakariya, Peter; Babuska, Tomas; Mundt, Miranda
DOI: 10.18126/yvgn-w386
Year: 2025

Data for Varying Kinetic Stability, Icosahedral Ordering, and Mechanical Properties of a Model Zr-Cu-Al Metallic Glass by Sputtering

Muley, Sachin V.; Cao, Chengrong; Chatterjee, Debaditya; Francis, Carter; Lu, Felix P.; Ediger, M. D.; Perpezko, John H.; Voyles, Paul M.
Organizations: MDF Open
DOI: 10.18126/xa3c-69j6
Year: 2020